AS/NZS 1462.8:2008 (R2017) Methods of test for plastics pipes and fittings - Method 8: Method of testing the leaktightness of assemblies

Abbreviation
AS/NZS 1462.8:2008
Valid from
29/06/2008

Information provider
Standards New Zealand,
Author
Standards New Zealand, Standards Australia
Information type
New Zealand Standard,


Description

This Standard specifies a method for testing the leaktightness of assemblies of plastics pipes and fittings with elastomeric sealing-ring socket joints or inspection openings, which may be subjected to diametric distortion and /or angular deflection.

Scope

This standard includes, but is not limited to -

  • (a) single sockets on pipes,
  • (b) double sockets,
  • (c) sockets on fittings, and
  • (d) inspection openings on fittings.

It is also applicable to elastomeric sealing-ring sockets made of other materials, e.g. ductile iron, intended for use with plastics piping.

For assistance with locating previous versions, please contact the information provider.
View on Information Provider website
For assistance with locating previous versions, please contact the information provider.
This resource is cited by:

AS/NZS 1462.8:2008 (R2017) Methods of test for plastics pipes and fittings - Method 8: Method of testing the leaktightness of assemblies

This document is CITED BY:

AS/NZS 1462.8:2008 (R2017) Methods of test for plastics pipes and fittings - Method 8: Method of testing the leaktightness of assemblies

Description

This Standard specifies a method for testing the leaktightness of assemblies of plastics pipes and fittings with elastomeric sealing-ring socket joints or inspection openings, which may be subjected to diametric distortion and /or angular deflection.

View on Information Provider website
AS/NZS 1462.8:2008 (R2017) Methods of test for plastics pipes and fittings - Method 8: Method of testing the leaktightness of assemblies
Description

This Standard specifies a method for testing the leaktightness of assemblies of plastics pipes and fittings with elastomeric sealing-ring socket joints or inspection openings, which may be subjected to diametric distortion and /or angular deflection.

View on Information Provider website
This resource does not cite any other resources.

AS/NZS 1462.8:2008 (R2017) Methods of test for plastics pipes and fittings - Method 8: Method of testing the leaktightness of assemblies

This resource does not CITE any other resources.
Feedback