ASTM B443-84 STANDARD SPECIFICATION FOR NICKEL-CHROMIUM- MOLYBDENUM-COLUMBIUM ALLOY (UNS NO6625) PLATE, SHEET, AND STRIP

Abbreviation
ASTM B443-84
Valid from
16/03/1984

Information provider
IHS Markit,
Author
American Society of Testing and Materials
Information type
ASTM Standard,
Format
PDF, HARD COPY,


Description

This specification covers rolled nickel-chromium-molybdenum-columbium alloy (UNS N06625) and nickel-chromium-molybdenum-silicon alloy (UNS N06219) plate, sheet, and strip. 

Alloy UNS N06625 products are furnished in two grades of different heat-treated conditions: 

  • Grade 1 (Annealed)-Material is normally employed in service temperatures up to 1100°F (593°C). 
  • Grade 2 (Solution Annealed)-Material is normally employed in service temperatures above 1100°F (593°C) when resistance to creep and rupture is required. 

For assistance with locating previous versions, please contact the information provider.
View on Information Provider website
For assistance with locating previous versions, please contact the information provider.
This resource is cited by:

ASTM B443-84 STANDARD SPECIFICATION FOR NICKEL-CHROMIUM- MOLYBDENUM-COLUMBIUM ALLOY (UNS NO6625) PLATE, SHEET, AND STRIP

This document is CITED BY:

ASTM B443-84 STANDARD SPECIFICATION FOR NICKEL-CHROMIUM- MOLYBDENUM-COLUMBIUM ALLOY (UNS NO6625) PLATE, SHEET, AND STRIP

Description

This specification covers rolled nickel-chromium-molybdenum-columbium alloy (UNS N06625) and nickel-chromium-molybdenum-silicon alloy (UNS N06219) plate, sheet, and strip. 

Alloy UNS N06625 products are furnished in two grades of different heat-treated conditions: 

  • Grade 1 (Annealed)-Material is normally employed in service temperatures up to 1100°F (593°C). 
  • Grade 2 (Solution Annealed)-Material is normally employed in service temperatures above 1100°F (593°C) when resistance to creep and rupture is required. 

View on Information Provider website
ASTM B443-84 STANDARD SPECIFICATION FOR NICKEL-CHROMIUM- MOLYBDENUM-COLUMBIUM ALLOY (UNS NO6625) PLATE, SHEET, AND STRIP
Description

This specification covers rolled nickel-chromium-molybdenum-columbium alloy (UNS N06625) and nickel-chromium-molybdenum-silicon alloy (UNS N06219) plate, sheet, and strip. 

Alloy UNS N06625 products are furnished in two grades of different heat-treated conditions: 

  • Grade 1 (Annealed)-Material is normally employed in service temperatures up to 1100°F (593°C). 
  • Grade 2 (Solution Annealed)-Material is normally employed in service temperatures above 1100°F (593°C) when resistance to creep and rupture is required. 

View on Information Provider website
This resource does not cite any other resources.

ASTM B443-84 STANDARD SPECIFICATION FOR NICKEL-CHROMIUM- MOLYBDENUM-COLUMBIUM ALLOY (UNS NO6625) PLATE, SHEET, AND STRIP

This resource does not CITE any other resources.
Feedback