ASTM B408-87 STANDARD SPECIFICATION FOR NICKEL-IRON-CHROMIUM ALLOY ROD AND BAR

Abbreviation
ASTM B408-87
Valid from
1/01/1987

Information provider
IHS Markit,
Author
American Society of Testing and Materials
Information type
ASTM Standard,
Format
PDF, HARD COPY,


Description

This specification covers UNS N08120, UNS N08800, UNS N08810, UNS N08811, and UNS N08890 in the form of hot-worked and cold-worked rod and bar.

Alloy UNS N08800 is normally employed in service temperatures up to and including 1100°F (593°C). Alloys UNS N08120, UNS N08810, UNS N08811, and UNS N08890 are normally employed in service temperatures above 1100°F (593°C) where resistance to creep and rupture is required, and they are annealed to develop controlled grain size for optimum properties in this temperature range. 

 

For assistance with locating previous versions, please contact the information provider.
View on Information Provider website
For assistance with locating previous versions, please contact the information provider.
This resource is cited by:

ASTM B408-87 STANDARD SPECIFICATION FOR NICKEL-IRON-CHROMIUM ALLOY ROD AND BAR

This document is CITED BY:

ASTM B408-87 STANDARD SPECIFICATION FOR NICKEL-IRON-CHROMIUM ALLOY ROD AND BAR

Description

This specification covers UNS N08120, UNS N08800, UNS N08810, UNS N08811, and UNS N08890 in the form of hot-worked and cold-worked rod and bar.

Alloy UNS N08800 is normally employed in service temperatures up to and including 1100°F (593°C). Alloys UNS N08120, UNS N08810, UNS N08811, and UNS N08890 are normally employed in service temperatures above 1100°F (593°C) where resistance to creep and rupture is required, and they are annealed to develop controlled grain size for optimum properties in this temperature range. 

 

View on Information Provider website
ASTM B408-87 STANDARD SPECIFICATION FOR NICKEL-IRON-CHROMIUM ALLOY ROD AND BAR
Description

This specification covers UNS N08120, UNS N08800, UNS N08810, UNS N08811, and UNS N08890 in the form of hot-worked and cold-worked rod and bar.

Alloy UNS N08800 is normally employed in service temperatures up to and including 1100°F (593°C). Alloys UNS N08120, UNS N08810, UNS N08811, and UNS N08890 are normally employed in service temperatures above 1100°F (593°C) where resistance to creep and rupture is required, and they are annealed to develop controlled grain size for optimum properties in this temperature range. 

 

View on Information Provider website
This resource does not cite any other resources.

ASTM B408-87 STANDARD SPECIFICATION FOR NICKEL-IRON-CHROMIUM ALLOY ROD AND BAR

This resource does not CITE any other resources.
Feedback