AS 1580.409.1-2002 (R2013) Paints and related materials - Methods of test - Resistance to mudcracking

Abbreviation
AS 1580.409.1-2002 (R2013)
Valid from
13/12/2002
Replaces
,

Information provider
Intertek Inform,
Author
Standards Australia
Information type
Australian Standard,
Format
PDF, HARD COPY,


Description

This Standard sets out a method for determining the resistance to mudcracking of an air-dried latex paint film, typically applied at 30–50 mm dry film thickness.

It provides a method for evaluating the tendency of paint coatings to crack in locations where there has been an excessive build-up of paint, e.g. in the corner of a room, particularly at ceilings and cornices, which occurs most commonly with flat paints.

Scope

 

For assistance with locating previous versions, please contact the information provider.
View on Information Provider website
For assistance with locating previous versions, please contact the information provider.
This resource is cited by:

AS 1580.409.1-2002 (R2013) Paints and related materials - Methods of test - Resistance to mudcracking

This document is CITED BY:

AS 1580.409.1-2002 (R2013) Paints and related materials - Methods of test - Resistance to mudcracking

Description

This Standard sets out a method for determining the resistance to mudcracking of an air-dried latex paint film, typically applied at 30–50 mm dry film thickness.

It provides a method for evaluating the tendency of paint coatings to crack in locations where there has been an excessive build-up of paint, e.g. in the corner of a room, particularly at ceilings and cornices, which occurs most commonly with flat paints.

View on Information Provider website
AS 1580.409.1-2002 (R2013) Paints and related materials - Methods of test - Resistance to mudcracking
Description

This Standard sets out a method for determining the resistance to mudcracking of an air-dried latex paint film, typically applied at 30–50 mm dry film thickness.

It provides a method for evaluating the tendency of paint coatings to crack in locations where there has been an excessive build-up of paint, e.g. in the corner of a room, particularly at ceilings and cornices, which occurs most commonly with flat paints.

View on Information Provider website